Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 34 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 260 °C
34 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 260 °C
34 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 260 °C
34 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Melt Flow 34 g/10 min

@Load 2.16 kg,
Temperature 260 °C
34 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D 1238
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East)
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Melt Flow 34 g/10 min

@Load 3.80 kg,
Temperature 230 °C
34 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238(I)
LG Chemical ALPHALAC SF510 HIPS
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
Melt Flow 34 g/10 min

@Load 10.0 kg,
Temperature 220 °C
34 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..
Melt Flow 34 g/10 min

@Load 10.0 kg,
Temperature 220 °C
34 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM Test
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..
Melt Flow 34 g/10 min

@Load 5.00 kg,
Temperature 230 °C
34 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound
Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance..
Melt Flow 34 g/10 min

@Load 10.0 kg,
Temperature 220 °C
34 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Denka CL-430 Transparent Resin Polymer (MABS) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Melt Flow 34 g/10 min

@Load 10.0 kg,
Temperature 220 °C
34 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-746 ABS - High Flow
High flow, medium impact
Copyright © lookpolymers.com All Rights Reserved