Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 260 °C |
33 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 260 °C |
33 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 260 °C |
33 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Asia Pacific) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Asia Pacific) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Europe-Africa-Middle East) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 250 °C |
33 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® 6134 NC010 PBT
(Unverified Data**) Crastin® 6134 NC010 is an unreinforced, medium viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 230 °C |
33 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 30 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Asia Pacific) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1880T PC Copolymer Lexan* EXL1880T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, transparent injection molding grade. This resin offers good low temperature (0 C) ductility in combination with very h.. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 330 °C |
33 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE1810T PC Copolymer (Europe-Africa-Middle East) Lexan* FXE1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection moldable grade. This specialty PC offers excellent processability, very high flow and improved ductility charac.. |
|||
Melt Flow | 33 g/10 min @Load 21.6 kg, Temperature 190 °C |
33 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene EX2S is a high density polyethylene with 1-Butene as co monomer. It is medium molar mass, low density grade with a narrow molar mass distribution, high rigidity, good tear strength. Applications: .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 250 °C |
33 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 250 °C |
33 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 250 °C |
33 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP821 PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in over-molding applications such as plugs, strain .. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 265 °C |
33 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Melt Flow | 33 g/10 min @Load 5.00 kg, Temperature 266 °C |
33 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Melt Flow | 33 g/10 min @Load 1.20 kg, Temperature 300 °C |
33 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Melt Flow | 33 g/10 min @Load 3.80 kg, Temperature 230 °C |
33 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Luriblend® HIPS E SL5 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant (5%)Appearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 260 °C |
33 g/10 min @Load 4.76 lb, Temperature 500 °F |
ISO 1133 |
Polyplastics TOPAS® 8007 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Water adsorption is small and barrier properties are good, making this grade particularly suitable for package applications for products that dislike moisture. Grade 8007 has lower coefficient of el.. |
|||
Melt Flow | 33 g/10 min @Load 21.6 kg, Temperature 190 °C |
33 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Melt Flow | 33 g/10 min @Load 2.16 kg, Temperature 190 °C |
33 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DSM Arnitel® EM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 33 g/10 min @Load 10.0 kg, Temperature 220 °C |
33 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |