Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 3.8 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 210 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 210 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th..
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Micropol Microlin ML90 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 250 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Xenoy® 5720U PBT+PC
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 250 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Melt Flow 3.8 g/10 min

@Load 2.16 kg,
Temperature 250 °C
3.8 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East)
Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY
Melt Flow 3.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 4001H3F
Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 3.8 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.8 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Diamond Polymers ABS 4001HH
Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved