Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Melt Flow | 3.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 9903D-10 Cyclic Olefin Copolymer (COC) TOPAS® 9903D-10 is a very low glass transition temperature (Tg=33°C) film extrusion grade. It is designed to deliver high shrinkage at low temperatures in shrink packaging applications. It is a mo.. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S140 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TW-17 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.7 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.7 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |