Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 9000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
Melt Flow | 3.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 95HC SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring.. |
|||
Melt Flow | 3.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 3.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 and ISO 1133 |
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin Product Description: Exxelor PE 1040 polymer resin is a maleic anhydride functionalized high density polyethylene, produced by reactive extrusion. It has been primarily designed to act as a coupli.. |