Polymer Property : Melt Flow = 29 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 200 °C
29 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce..
Melt Flow 29 g/10 min

@Load 5.00 kg,
Temperature 200 °C
29 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4401R PPC+PC
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East)
LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4404 PPC+PC
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Melt Flow 29 g/10 min

@Load 2.16 kg,
Temperature 330 °C
29 g/10 min

@Load 4.76 lb,
Temperature 626 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East)
High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi..
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 300 °C
29 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® DMX9254 PC
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 300 °C
29 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 300 °C
29 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Melt Flow 29 g/10 min

@Load 21.6 kg,
Temperature 190 °C
29 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
SABIC B5429/B5429A High Density Polyethylene for Blow Molding
Product Description: B5429 Series grades are medium molecular weight High Density Polyethylene copolymer. They are primarily intended for blow molding articles of small sizes. B5429 series grades..
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 300 °C
29 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East)
Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b..
Melt Flow 29 g/10 min

@Load 1.20 kg,
Temperature 300 °C
29 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific)
Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di..
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 420 °C
29 g/10 min

@Load 22.0 lb,
Temperature 788 °F
ASTM D1238
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled  (discontinued **)
AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU..
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 220 °C
29 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 220 °C
29 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Melt Flow 29 g/10 min

@Load 21.6 kg,
Temperature 190 °C
29 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil HDPE HYA 600 High Density Polyethylene Resin
Product Description: HYA 600 is a general purpose HDPE resin, characterized by very easy processability, an excellent balance of rigidity and impact strength and a good ESCR.Availability: Africa & M..
Melt Flow 29 g/10 min

@Load 10.0 kg,
Temperature 220 °C
29 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Melt Flow 29 g/10 min

@Load 21.6 kg,
Temperature 190 °C
29 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM-D1238
Braskem HB0454HR HDPE Blow Molding Polyethylene Copolymer
HB0454HR is a high-density polyethylene copolymer resin with average molecular weight produced by the Unipol® process. A bottle made with HB0454HR shows excellent processability, color, and superfi..