Polymer Property : Melt Flow = 21.6 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 21.6 g/10 min

@Load 3.80 kg,
Temperature 230 °C
21.6 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific)
ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses.
Melt Flow 21.6 g/10 min

@Load 10.0 kg,
Temperature 220 °C
21.6 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Luran® 378 P Crystal Clear Transparent SAN
Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS