Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 20.52 g/10 min @Load 10.0 kg, Temperature 220 °C |
20.52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® 348 Q Crystal Clear Transparent 77850 SAN Description: Highly transparent grade with low natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Melt Flow | 20.52 g/10 min @Load 10.0 kg, Temperature 220 °C |
20.52 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® 348 Q Transparent SAN Description: Highly transparent grade with light natural color.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |