Physical Properties Metric English Comments
Melt Flow 2.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Network Polymers SAN 290 Light Blue Tint
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Melt Flow 2.4 - 3.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 - 3.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1283/L
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 2.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Kuraray SEPTON® S2007 Thermoplastic Rubber
SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi..
Melt Flow 2.4 g/10 min

@Load 6.60 kg,
Temperature 295 °C
2.4 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D 1238
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East)
High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East..
Melt Flow 2.4 g/10 min

@Load 6.60 kg,
Temperature 295 °C
2.4 g/10 min

@Load 14.6 lb,
Temperature 563 °F
ASTM D 1238
SABIC Innovative Plastics Ultem UR9076LG PEI
Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)  (Unverified Data**)
Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi..
Melt Flow 2.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer
Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod..
Melt Flow 2.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DuPont Performance Polymers Delrin® FG150 NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact ApplicationsDelrin FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. I..
Melt Flow 2.4 - 5.2 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.4 - 5.2 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
BASF Ecovio® C2224 F Blend Biodegradable Polyester
Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci..
Melt Flow 2.4 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.4 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Pellets; ASTM D-1238-94a
Multibase Multi-ABS 1030 White
Data provided by Multibase.