Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.16 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.16 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Terlux® 2802 TR Q434 Transparent MABS Description: Terlux® 2802 TR Q434 is a new grade with enhanced toughness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |