Polymer Property : Melt Flow = 17.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 17.4 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17.4 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP781 PPE-TPE
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Melt Flow 17.4 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17.4 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Asia Pacific)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Melt Flow 17.4 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17.4 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL WCP781 PPE-TPE (Europe-Africa-Middle East)
Flexible PPE-TPE injection grade. Low specific gravity with very good halogen free flame retardant performance. Suitable for over-molding applications such as plugs, strain relief's, and connecto..
Melt Flow 17.4 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.4 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP D452 PC COPOLYMER (Asia Pacific)
LNP* Thermocomp* D452 (or EXTC8202) is a compound based on SABIC unique Polycarbonate copolymer resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, ..
Copyright © lookpolymers.com All Rights Reserved