Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 220 °C |
15 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 220 °C |
15 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 220 °C |
15 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 220 °C |
15 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 220 °C |
15 g/10 min @Load 22.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 260 °C |
15 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 220 °C |
15 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 260 °C |
15 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Melt Flow | 15 g/10 min @Load 3.80 kg, Temperature 230 °C |
15 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Melt Flow | 15 g/10 min @Load 3.80 kg, Temperature 280 °C |
15 g/10 min @Load 8.38 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 15 g/10 min @Load 3.80 kg, Temperature 280 °C |
15 g/10 min @Load 8.38 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific) Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 250 °C |
15 g/10 min @Load 11.0 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 265 °C |
15 g/10 min @Load 4.76 lb, Temperature 509 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 265 °C |
15 g/10 min @Load 4.76 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 200 °C |
15 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM Test |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 280 °C |
15 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 280 °C |
15 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 280 °C |
15 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Melt Flow | 15 g/10 min @Load 21.6 kg, Temperature 190 °C |
15 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis HC101BF Polypropylene Homopolymer HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa.. |
|||
Melt Flow | 15 g/10 min @Load 5.00 kg, Temperature 230 °C |
15 g/10 min @Load 11.0 lb, Temperature 446 °F |
Volume Resistivity 10 ohm-cm |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very .. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 240 °C |
15 g/10 min @Load 4.76 lb, Temperature 464 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 15 g/10 min @Load 21.6 kg, Temperature 190 °C |
15 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Melt Flow | 15 g/10 min @Load 10.0 kg, Temperature 265 °C |
15 g/10 min @Load 22.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xylex HX7409HP PC+POLYESTER (Asia Pacific) Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 190 °C |
15 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene V1160 High Density Polyethylene CHARACTERISTICS: GOOD FLOWABILITYAPPLICATIONS: INJECTION MOLDING FOR LIGHT WEIGHT HOUSEHOLDS, TOYS, FOOD CONTAINERS, COSMETICS CLOSURES, DISPOSABLE ARTICLES, LARGE MOLDING AND COMPLICATED PARTS |
|||
Melt Flow | 15 g/10 min @Load 21.6 kg, Temperature 190 °C |
15 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® ZB 20 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 15 g/10 min @Load 2.16 kg, Temperature 240 °C |
15 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang. |