Physical Properties Metric English Comments
Melt Flow 137 g/10 min

@Load 10.0 kg,
Temperature 220 °C
137 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238(G)
LG Chemical ALPHALAC SF510 HIPS