Physical Properties Metric English Comments
Melt Flow 12.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® IFX2420Z PC (Asia Pacific)
Lexan* IFX2420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware applications specifically for welding. This grades ..
Melt Flow 12.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® IFX6420Z PC (Asia Pacific)
Lexan* IFX6420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm..
Melt Flow 12.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) MF3313 High Density Polyethylene
MF3313 is a high molecular weight high density polyethylene . Applications: extrusion, film, blown, bags, and density modifies.Information provided by Iran Petrochemical Commercial Co.
Melt Flow 12.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
12.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su..
Melt Flow 12.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
12.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
SABIC Innovative Plastics Ultem XH6050F PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was ..
Melt Flow 12.5 g/10 min

@Load 6.60 kg,
Temperature 367 °C
12.5 g/10 min

@Load 14.6 lb,
Temperature 693 °F
ASTM D 1238
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
Melt Flow 12.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
12.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR
Information provided by Samsung Cheil Industries.
Melt Flow 12.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
12.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® HN-3104 PC, 10% Glass Filled FR
Information provided by Samsung Cheil Industries.
Melt Flow 12.5 g/10 min

@Load 2.16 kg,
Temperature 240 °C
12.5 g/10 min

@Load 4.76 lb,
Temperature 464 °F
ISO 1133
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Melt Flow 12.5 g/10 min

@Load 2.16 kg,
Temperature 240 °C
12.5 g/10 min

@Load 4.76 lb,
Temperature 464 °F
ISO 1133
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers