Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 110 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 110 g/10 min

@Load 5.00 kg,
Temperature 200 °C
110 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE)
Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex..
Melt Flow 110 g/10 min

@Load 1.00 kg,
Temperature 235 °C
110 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
Network Polymers Softflex® 0250
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Melt Flow 110 g/10 min

@Load 5.00 kg,
Temperature 266 °C
110 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East)
VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin.
Melt Flow 110 g/10 min

@Load 1.20 kg,
Temperature 190 °C
110 g/10 min

@Load 2.65 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil EXXELOR™ PO 1020 Maleic anhydride functionalized polypropylene
Product Description: Exxelor PO 1020 polymer resin is a high performance maleic anhydride fuctionalized homopolypropylene produced by reactive extrusion. It has been primarily designed to add polari..
Copyright © lookpolymers.com All Rights Reserved