Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 10.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 10.5 - 13.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10.5 - 13.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4131L (314F4) Linear Low Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 10.5 - 21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10.5 - 21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6252J (526F2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 10.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® I2220 PC
General purpose polycarbonate with melt flow rate of 10.5.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 10.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® IR2240 PC
UL rated HB. 200 series recommended when V-2 rating required. Nonhalogenated. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for..
Melt Flow 10.5 - 21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10.5 - 21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 4252J (524F2) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 10.5 g/10 min

@Load 2.16 kg,
Temperature 210 °C
10.5 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Melt Flow 10.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
10.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Melt Flow 10.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
10.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Diamond Polymers SAN 268 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved