Polymer Property : Melt Flow = 1.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE)
Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV..
Melt Flow 1.4 g/10 min

@Load 5.00 kg
1.4 g/10 min

@Load 11.0 lb
ASTM D 1238
Total Finathene® 6002 HDPE, blow molding, pipe  (discontinued **)
FINATHENE® 6002 is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® 6002 has been especially developed for the manufacturing of toys and of b..
Melt Flow 1.4 g/10 min

@Load 5.00 kg
1.4 g/10 min

@Load 11.0 lb
ISO 1133
Total Lacqtene® 2005 TN 59 HDPE pipe  (discontinued **)
LACQTENE® 2005 TN 59 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2005 TN 59 is best processed between 190 and 230°C.Informa..
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA S610
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 1.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA S710
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 and ISO 1133
ExxonMobil Exxelor™ PE 1040 High Density Polyethylene Resin
Product Description: Exxelor PE 1040 polymer resin is a maleic anhydride functionalized high density polyethylene, produced by reactive extrusion. It has been primarily designed to act as a coupli..