Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.90 - 1.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 - 1.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4121N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.90 - 1.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 - 1.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4122N (22401) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.80 - 1.3 g/10 min @Load 2.16 kg, Temperature 170 °C |
0.80 - 1.3 g/10 min @Load 4.76 lb, Temperature 338 °F |
|
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |