Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.34 g/10 min @Load 5.00 kg |
0.34 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total Finathene® 2344 HDPE film
(discontinued **) Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |
|||
Melt Flow | 0.34 g/10 min @Load 5.00 kg |
0.34 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Melt Flow | 0.34 g/10 min @Load 5.00 kg |
0.34 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Melt Flow | 0.34 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.34 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y.. |
|||
Melt Flow | 0.34 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.34 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta.. |
|||
Melt Flow | 0.34 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.34 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con.. |