Polymer Property : Melt Flow = 0.34 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.34 g/10 min

@Load 5.00 kg
0.34 g/10 min

@Load 11.0 lb
ASTM D 1238
Total Finathene® 2344 HDPE film  (discontinued **)
Applications: Trash can liners, merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines.
Melt Flow 0.34 g/10 min

@Load 5.00 kg
0.34 g/10 min

@Load 11.0 lb
ASTM D 1238
Total Finathene® 3344N Natural HDPE pipe grade  (discontinued **)
Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To..
Melt Flow 0.34 g/10 min

@Load 5.00 kg
0.34 g/10 min

@Load 11.0 lb
ASTM D 1238
Total HP 401N Natural HDPE, pipe
Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T..
Melt Flow 0.34 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer
GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y..
Melt Flow 0.34 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene
Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta..
Melt Flow 0.34 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.34 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene
Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con..