Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.10 - 0.20 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.10 - 0.20 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4252A (524H1) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |