Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 46.56 - 62.08 cc/m²/day | 2.998 - 3.998 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® Emblem™ 1500 Clear Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydr.. |
|||
Oxygen Transmission Rate | 46.56 - 62.08 cc/m²/day | 2.998 - 3.998 cc/100 in²/day | 77°F / 0% / RH; ASTM D3985 |
Honeywell Capran® Emblem™ 1500M M-Coated Bi-Axially Oriented Nylon Film Description: Capran® Emblem™ 1500M is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hyd.. |