Physical Properties Metric English Comments
Oxygen Transmission Rate 250 cc/m²/day

@Thickness 0.00100 mm
16.1 cc/100 in²/day

@Thickness 0.0000394 in
85% RH; ASTM D398
Solvay Specialty Polymers Ixan® SGA-1 Polyvinylidene Chloride (PVDC)
IXAN® SGA-1 is a self-adhesive coat for use on aluminum, steel and plastic films, metalized or not. This universal grade may also be used as an adhesion primer for laminating or coating on plasti..
Oxygen Transmission Rate 250 cc/m²/day
16.1 cc/100 in²/day
23°C/85%r.h.; DIS 15105-1/-2
EMS-Grivory Grivory® CA 6 E PA*
Product description: Grilon CA 6 E is a non-extracted copolyamide with a low melting point. Grilon CA 6 E characterizes itself through the following properties Very high flexibility and toughnessVer..
Oxygen Transmission Rate 250 cc/m²/day
16.1 cc/100 in²/day
25°C, 1.0 µm, 85% RH
Solvay Specialty Polymers Ixan® SGA-1 Polyvinylidene Chloride (PVDC)  (Unverified Data**)
IXAN® SGA-1 is a self-adhesive coat for use on aluminium, steel and plastic films, metallised or not. This universal grade may also be used as an adhesion primer for laminating or coating on plasti..