Polymer Property : Oxygen Transmission Rate = 10000 cc/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate >= 10000 cc/m²/day
>= 644 cc/100 in²/day
25°C, 0% RH; 25um; ASTM D1434
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating
The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a..