Physical Properties Metric English Comments
Water Vapor Transmission 7.20 g/m²/day
0.464 g/100 in²/day
at 100°F, 90% RH; ASTM F1249-90
Dow Saran® 18L Clear Plastic Barrier Film
Saran™ 18L is a clear biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow
Water Vapor Transmission 7.20 g/m²/day
0.464 g/100 in²/day
at 100°F, 90% RH; ASTM F1249-90
Dow Saran® 18L-WP White Plastic Barrier Film
Saran™ 18L-WP is a white biaxially oriented monolayer barrier film, preshrunk for lamination applications. It is available in 75 gauge, as single or double wound rolls.Information provided by Dow