Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 6.98 g/m²/day @Temperature 37.8 °C |
0.450 g/100 in²/day @Temperature 100 °F |
100% RH; ASTM F1249 |
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp.. |