Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Water Vapor Transmission = 6.20 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
100°F; E 96/66
Total Finathene® 1288 HDPE film  (discontinued **)
Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti..
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
100°F; E 96/66
Total Finathene® 6450 HDPE film  (discontinued **)
Applications: overwrap, food packaging, coextrusion, extrusion coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lin..
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
100% Humidity; ASTM F372
LyondellBasell Plexar® PX3060 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and ..
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
at 100°F, 90% RH; ASTM F1249-90
Dow Saran® 28 Clear Plastic Barrier Film
Saran™ 28 is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double wound rolls.Information prov..
Water Vapor Transmission 6.20 g/m²/day
0.399 g/100 in²/day
ASTM E96 Procedure E
DuPont™ Sclairfilm® BL-1 LLDPE Film, PVDC Coated, 51 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A one-side PVDC-coated LLDPE sealant film, which provides excellent barrier properties, while retaining the outstanding physical and seal strength characte..
Copyright © lookpolymers.com All Rights Reserved