Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 4.70 g/m²/day | 0.303 g/100 in²/day | ASTM E96 Procedure E |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Water Vapor Transmission | 4.70 g/m²/day | 0.303 g/100 in²/day | ASTM E96 Procedure E |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Water Vapor Transmission | 4.70 g/m²/day | 0.303 g/100 in²/day | ASTM E96 Procedure E |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Water Vapor Transmission | 4.70 g/m²/day | 0.303 g/100 in²/day | ASTM E96 Procedure E |
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A general purpose linear low density polyethylene sealant film designed for less critical sealing applications than type SL. It provides good heat seal an.. |
|||
Water Vapor Transmission | 4.70 g/m²/day | 0.303 g/100 in²/day | ASTM E96 Procedure E |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Water Vapor Transmission | 4.70 g/m²/day @Temperature 37.8 °C |
0.303 g/100 in²/day @Temperature 100 °F |
90% RH; thickness not specified; ASTM E96 |
Total PPH 3271 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – FINA 3271 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock –.. |
|||
Water Vapor Transmission | 4.70 g/m²/day @Temperature 37.8 °C |
0.303 g/100 in²/day @Temperature 100 °F |
90% RH; thickness not specified; ASTM E96 |
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Water Vapor Transmission | 4.70 g/m²/day @Temperature 37.8 °C |
0.303 g/100 in²/day @Temperature 100 °F |
90% RH; thickness not specified; ASTM E96 |
Total PPH 3276 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals – Fina 3276 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock .. |
|||
Water Vapor Transmission | 4.70 - 30.0 g/m²/day | 0.303 - 1.93 g/100 in²/day | Average value: 9.30 g/m²/day Grade Count:24 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Water Vapor Transmission | 4.70 g/m²/day | 0.303 g/100 in²/day | ASTM E96 Procedure E |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |