Polymer Property : Water Vapor Transmission = 1.20 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 1.20 g/m²/day
0.0773 g/100 in²/day
ASTM D1653
3M Scotchkote™ 162HB Epoxy Coating
3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w..