Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 10.9 g/m²/day @Thickness 0.0254 mm |
0.702 g/100 in²/day @Thickness 0.00100 in |
ASTM F1249 |
Total 9458 HDPE Film Grade Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba.. |
|||
Water Vapor Transmission | 10.9 g/m²/day | 0.702 g/100 in²/day | 38°C, 90% RH; ExxonMobil Method |
ExxonMobil Bicor® 50 LBW OPP Film Product Description: Bicor LBW is a two-sided treated, slip modified, non-heat sealable OPP film designed for use as the outside web of a lamination. The print surface is treated and can be printed .. |