Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 10.5 g/m²/day | 0.676 g/100 in²/day | |
LG Chemical LUTENE FB3000 LDPE Extrusion of Blown Film Description: LUTENE FB3000 is mainly intended for the extrusion of blown film with high mechanical property for the clarity bags in all thickness. LUTENE FB3000 have high mechanical property and ena.. |
|||
Water Vapor Transmission | 10.5 g/m²/day | 0.676 g/100 in²/day | 1 atm, 38°C, 100% RH; ASTM D1249 |
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |