Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 9.31 - 12.42 g/m²/day | 0.600 - 0.7998 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 1230 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 1230 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Water Vapor Transmission | 9.31 - 12.42 g/m²/day | 0.600 - 0.7998 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film
(discontinued **) Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many .. |
|||
Water Vapor Transmission | 9.31 - 12.42 g/m²/day | 0.600 - 0.7998 g/100 in²/day | 100°F / 100%RH); ASTM F1249 |
Honeywell Capran® Emblem™ 2530 Bi-Axially Oriented Nylon Film
(discontinued **) Description: Capran® Emblem™ 2530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbo.. |
|||
Water Vapor Transmission | 9.31 g/m²/day | 0.600 g/100 in²/day | 100°F; E 96/66 |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Water Vapor Transmission | 9.31 g/m²/day @Temperature 38.0 °C |
0.600 g/100 in²/day @Temperature 100 °F |
90% RH; ASTM F1249 |
DuPont Teijin Films Mylar® CL Polyester Film, 50 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |