Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.420 g/m²/day | 0.0270 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® 11A(0.60 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Water Vapor Transmission | 0.420 g/m²/day | 0.0270 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® 33C (0.75 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Water Vapor Transmission | 0.420 g/m²/day | 0.0270 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag.. |