Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.202 g/m²/day | 0.0130 g/100 in²/day | 104°F (40°C) / 75%RH; ASTM F1249 |
Honeywell ACLAR® SupRx 900 CTFE Homopolymer, Barrier Film Description: ACLAR® SupRx 900 is a .9 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |
|||
Water Vapor Transmission | 0.202 g/m²/day @Temperature 38.0 °C |
0.0130 g/100 in²/day @Temperature 100 °F |
90% RH; ExxonMobil Method |
ExxonMobil Metallyte™ 18MM383 OPP Film Product Description: A biaxially oriented very high barrier metalized polypropylene film. This film offers an outstanding moisture barrier and a broad seal range surface on the other side. This film.. |