Physical Properties | Metric | English | Comments |
---|---|---|---|
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 430 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
4300 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Carbon Dioxide Transmission | 430 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
4300 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 430 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
4300 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Carbon Dioxide Transmission | 430 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
4300 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Carbon Dioxide Transmission | 430 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
4300 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 3152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Carbon Dioxide Transmission | 429 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
1090 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
16900 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |