Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 9.41 bar @Temperature 20.0 °C |
7060 torr @Temperature 68.0 °F |
Vapor Density=1.48 |
LG Chemical Propylene Physical Properties: Highly reactive in polymerization and addition reaction. and Colorless, Narcotic gasStructure & Characteristics: Structure and characteristics: CH2=CH-CH3. A colorless inflammab.. |