Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.685 bar | 514 torr | Average value: 0.685 bar Grade Count:9 |
Overview of materials for Expanded Polystyrene (EPS) This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® F 215 N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing a uniformly distributed ?ame retardant (blowing agent: pentane)Remarks: For the manufacture of flame-retardant foams.Applications: Blocks, insula.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® F 315-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® F 395 -N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® P 326 M Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded parts with very good mechanical .. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® P 570 Expandable Polystyrene Additive Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Only foamed particles, good foaming capacity.Applications: For the production of expanded particles as a filling material .. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® F 295-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkageApplicati.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® F 495-N Expandable Polystyrene Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane)Remarks: Production of flame-retardant foams displaying low post-shrinkage.Applicat.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® P 326 C Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Molded partsInformation provided by BAS.. |
|||
Vapor Pressure | 0.685 bar @Temperature 25.0 °C |
514 torr @Temperature 77.0 °F |
|
BASF Styropor® P 426 Expandable Polystyrene Description: Expandable polystyrene (EPS) (blowing agent: pentane).Remarks: Good foaming capacity, energy-saving processing and short cycle time.Applications: Thin-walled molded parts.Information pr.. |