Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.568 bar @Temperature 20.0 °C |
426 torr @Temperature 68.0 °F |
Vapor Density=2.5 |
LG Chemical C5 Product Structure & Characteristics: Obtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process, and C5 content is higher than 95%. Although it is in liqui.. |
|||
Vapor Pressure | 0.568 bar @Temperature 20.0 °C |
426 torr @Temperature 68.0 °F |
Vapor Density=2.5 |
LG Chemical n-Pentane CH3CH2CH3. Saturated hydrocarbon fatty acid. Dissolved in crude oil. Colorless gas with slightly characteristic odor, and is heavier than air.Uses: Used as an EPS foaming agent named 'styrofoam' by .. |