Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | <= 0.000100 bar | <= 0.0750 torr | |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |