Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0000133 bar @Temperature 25.0 °C |
0.00998 torr @Temperature 77.0 °F |
|
BASF Lupranate® T80 Toluene Diisocyanate Description: Lupranate® T80 toluene diisocyanate (TDI) is an 80% - 20% mixture of the 2,4 and 2,6 isomers of toluene diisocyanate. This product is used in the preparation of polyurethane foams, pre.. |
|||
Vapor Pressure | 0.0000133 bar @Temperature 25.0 °C |
0.00998 torr @Temperature 77.0 °F |
|
BASF Lupranate® TF2115 Isocyanate Description: Lupranate® TF2115 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric-MDI) enriched with monomeric-MDI.Information provided by BASF |
|||
Vapor Pressure | 0.0000133 bar @Temperature 25.0 °C |
0.00998 torr @Temperature 77.0 °F |
|
BASF Lupranate® 8020 Isocyanate Description: Lupranate® 8020 Isocyanate is an 80:20 weight percent combination of toluene diisocyanate (TDI) and polymethylene polyphenylisocyanate (polymeric MDI). This product is used in the prep.. |