Physical Properties Metric English Comments
Vapor Pressure <= 0.000100 bar
<= 0.0750 torr
BASF Palamoll® 656 Polymeric Plasticizer
Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro..