Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 251 microns | 9.90 mil | |
Hexcel® HexForce™ 286 Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 251 microns | 9.90 mil | ASTM D3752 |
3M 8777 Sealing Tape 3M™ Sealing Tape 8887 is a self-adhered, waterproof membrane designed for sealing on difficult to stick to surfaces. This product has a unique acrylic pressure sensitive adhesive that aggressively .. |