Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 2160 microns | 85.0 mil | |
SMAC SMACFOAM® 1250S-01 Damping Material SMAC has developed sound absorbing material dedicated to be used in aerospace and defense activities thanks to its good acoustic properties, its lightweight and its fire resistance properties.Uses: .. |
|||
Thickness | 2160 microns | 85.0 mil | Overall |
Arlon 10842S085 Fully Cured, Unsupported Silicone Rubber Product Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by AR.. |
|||
Thickness | 2160 microns | 85.0 mil | Rubber |
Arlon 30400N085 0.085" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |
|||
Thickness | 2160 microns | 85.0 mil | ASTM D3752 |
3M 528 Impact Stripping Tape 3M™ Impact Stripping Tape 528 is a thick impact stripping tape used to provide excellent surface protection during plastic media blast (PMB) paint stripping operations.Information provided by 3M |
|||
Thickness | 2160 microns | 85.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Thickness | 2160 microns | 85.0 mil | Rubber |
Arlon 30850S085 0.085" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |