Polymer Property : Thickness = 787 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 787 - 1140 microns
31.0 - 45.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Thickness 787 - 1140 microns
31.0 - 45.0 mil
Range of Thicknesses Available
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
Thickness 787 microns
31.0 mil
3M Bumpon™ SJ5832 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Thickness 787 microns
31.0 mil
3M Bumpon™ SJ6032 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Thickness 787 microns
31.0 mil
3M 4032 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Thickness 787 microns
31.0 mil
3M 4052 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..
Thickness 787 microns
31.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat..
Thickness 787 microns
31.0 mil
3M Bumpon™ SJ6232 Resilient Rollstock
3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M
Thickness 787 microns
31.0 mil
Liner
3M FP018 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
Thickness 787 microns
31.0 mil
3M 4658F Double Coated Removable Foam Tape with Adhesive 100
3M™ Double Coated Removable Foam Tape 4658F is a clear, double coated acrylic foam tape that removes cleanly from many surfaces. 3M™ Adhesive 100 is a firm acrylic adhesive system that offers high..
Thickness 787 microns
31.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..