Physical Properties Metric English Comments
Thickness 180 - 1020 microns
7.09 - 40.2 mil
Parker Chomerics CHO-BOND® 1016 Electrically Conductive Sealant
Description: CHO-BOND 1016 sealant is an electrically conductive, one-component RTV silicone which provides both environmental sealing and EMI shielding. This seal, filled with nickel-plated graphit..
Thickness 180 - 12700 microns
7.09 - 500 mil
Parker Chomerics Duralan II™ AR Polycarbonate Unshielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability..
Thickness 180 - 12700 microns
7.09 - 500 mil
Parker Chomerics Duralan II™ P Polycarbonate Unshielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate. A unique feature of Parker Chomerics window products is the capability..
Thickness 180 - 12700 microns
7.09 - 500 mil
Average value: 4290 microns Grade Count:5
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Thickness 180 microns
7.09 mil
Isoflon Tisoflon® 6S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.