Physical Properties Metric English Comments
Thickness 1270 microns
50.0 mil
nom
Mid-Mountain Materials SILTEX® 36 Amorphous Silica Textile
Description: SILTEX is a family of high performance textile fabric that is comprised of high purity, high strength amorphous silica fibers, woven into a strong, flexible fabric designed for use wher..
Thickness 1270 microns
50.0 mil
Zircar Ceramics APA-2 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-2 is a flexible un-bonded sheet that contains no organic binder. Applications include thermal insulation in low ..
Thickness 1270 microns
50.0 mil
Overall; Arlon SQA-TMS-003
Arlon 10322B050 0.050" (1.27 mm) Fully Cured Silicone Rubber with Polyethylene Liner
Design/Construction:Liner: Polyethylene Material: Fully Cured Silicone RubberProduct Use: Anti-Static Vacuum BaggingAppearance: Black elastomeric sheetThis data represents typical values for the pro..
Thickness 1270 microns
50.0 mil
Silicone; Arlon SQA-TMS-003
Arlon 32980X050 0.050" Uncured Silicone Rubber on Polyester Film
Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material..
Thickness 1270 microns
50.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi..
Thickness 1270 microns
50.0 mil
Rubber; Arlon SQA-TMS-003
Arlon E950-10RXX-M8 0.050" (1.27 mm) Cured Silicone Rubber with PSA liner
Description: 1 inch wide, 50 mil thick, Red, Rectangular cross-section, Fully cured silicone interleaved with 0.002” PSA liner. Product is supplied in various roll lengths and the xx in the product..
Thickness 1270 microns
50.0 mil
Rubber; Arlon SQA-TMS-003
Arlon LW50125R##-P1 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll lengt..
Thickness 1270 microns
50.0 mil
Rubber; Arlon SQA-TMS-003
Arlon LW50125Rxx-P0 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubber Cross-Se..
Thickness 1270 microns
50.0 mil
Rubber; Arlon SQA-TMS-003
Arlon LW5015Y##-M1 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.5 inch wide, 50 mil thick, Yellow, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll len..
Thickness 1270 microns
50.0 mil
Arlon SQA-TMS-003
Arlon R35232B050 0.050" Fully Cured, Static Dissipating Silicone Rubber
Fully cured, unsupported, static dissipating silicone.Design/Construction:Liner: 3 mil PolyethyleneProduct: Fully Cured Silicone RubberCarrier: N/AThis data represents typical values for the produc..
Thickness >= 1270 microns
>= 50.0 mil
estimated wet film thickness
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Thickness >= 1270 microns
>= 50.0 mil
recommended dry film thickness
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Thickness >= 1270 microns
>= 50.0 mil
estimated wet film thickness
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
Thickness >= 1270 microns
>= 50.0 mil
recommended dry film thickness
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..