Physical Properties Metric English Comments
Thickness 147 microns
5.80 mil
Hexcel® HexForce™ 6557 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 147 microns
5.80 mil
Total; ASTM D3752
3M 363LC High Temperature Aluminum Foil/Glass Cloth Tape
3M™ High Temperature Aluminum Foil/Glass Cloth Tape 363LC can be used as a high temperature, heat reflective, protective wrap for certain cables and other components in aerospace and industrial app..
Thickness 147 microns
5.80 mil
Prepreg thickness - glass style 2112
Arlon 25FR Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
Thickness 147 microns
5.80 mil
Prepreg thickness - glass style 2112
Arlon 25N Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
Thickness 147 microns
5.80 mil
Tape
3M 9425 Repositionable Tape
3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M
Thickness 147 microns
5.80 mil
Liner
3M FM118B Indoor UL Recognized MC Polyester Label Products
3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po..
Thickness 147 microns
5.80 mil
Liner
3M FM12B Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
Thickness 147 microns
5.80 mil
Liner
3M FM14B Indoor UL Recognized Computer Imprintable Clear Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Thickness 147 microns
5.80 mil
Liner
3M FM15B Indoor UL Recognized Computer Imprintable Silver Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a..
Thickness 147 microns
5.80 mil
Liner
3M FV06B Semi-Rigid White Vinyl Label Product
3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general..
Thickness 147 microns
5.80 mil
Liner
3M FV09B Soft Translucent Vinyl Label Products
3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high..
Thickness 147 microns
5.80 mil
without adhesive
3M Scotchcal™ IJ66 Perforated Window Graphic Film
Film IJ66 is a 5.8-mil vinyl with a 40% perforated pattern and a removable, pressure-sensitive adhesive. This film allows a full image to be seen on the outside of a window while allowing viewing th..
Thickness 147 microns
5.80 mil
Liner
3M FM16B Indoor UL Recognized Computer Imprintable White Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Thickness 147 microns
5.80 mil
ASTM D3652
3M 1900 Specialty High Temperature Masking Tape
3M™ Value Duct Tape 1900 is a conformable cloth duct tape made with polyethylene film over cloth scrim and rubber adhesive. A good choice for non-critical applicationsInformation provided by 3M
Thickness 147 microns
5.80 mil
Backing; ASTM D3752
3M 5153 PTFE Glass Cloth Tape
3M™ PTFE Glass Cloth Tape 5151 is constructed using (PTFE) polytetra-fluoroethylene impregnated glass cloth and silicone adhesive. This tape is used in many applications requiring high temperature ..
Copyright © lookpolymers.com All Rights Reserved