Polymer Property : Thickness = 300 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 15.0 - 300 microns
0.591 - 11.8 mil
Average value: 52.7 microns Grade Count:109
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a..
Thickness 50.0 - 300 microns
1.97 - 11.8 mil
LG Chemical LUTENE FB0300 LDPE Blown Film Grade
Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e..
Thickness 50.0 - 300 microns
1.97 - 11.8 mil
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade
Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific..
Thickness 30.0 - 300 microns
1.18 - 11.8 mil
possible range, depending on extrusion conditions
Total EVA 1003 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1003 VN 4 is made by a high pressure tubular process. Grade for flexible films with very high transparency and outstanding mechanical properties. Contains an antioxidant.Application examples: ..
Thickness 45.0 - 300 microns
1.77 - 11.8 mil
possible range, depending on extrusion conditions
Total EVA 1005 VN 2 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 2 is made by a high pressure tubular process. Grade for transparent and resistant films. Contains an antioxidant.Application examples: Stretch, coextrusion, frozen food, agriculture fi..
Thickness 30.0 - 300 microns
1.18 - 11.8 mil
possible range, depending on extrusion conditions
Total EVA 1005 VN 4 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 4 is made by a high pressure tubular process. Grade for flexible films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: High strengt..
Thickness 25.0 - 300 microns
0.984 - 11.8 mil
possible range, depending on extrusion conditions
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa..
Thickness 25.0 - 300 microns
0.984 - 11.8 mil
possible range, depending on extrusion conditions
Total EVA 1005 VN 5 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1005 VN 5 is made by a high pressure tubular process. Grade for films with high transparency and good mechanical properties. Contains an antioxidant.Application examples: Coextrusion, stretch ..
Thickness 5.00 - 300 microns
0.197 - 11.8 mil
Average value: 35.2 microns Grade Count:16
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Thickness 12.7 - 300 microns
0.500 - 11.8 mil
Average value: 49.9 microns Grade Count:219
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..