Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-1042 LLDPE Packaging Film Resin, Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown clarity film resin. Films made from LL-1042 have very good tensile properties and toughness in addition to good clarity The good st.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-1108 LLDPE Film/Sandwich Bag Resin; 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin formulated with high slip, medium antiblock and processing aid for narrow die gap extrusion. Films made from LL-1108 have.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Escorene® LL-3218 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3218 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
Honeywell ETFE EX30 Mono-Axially Oriented, ETFE Film
(discontinued **) Description: ETFE EX30 is a 1.2 mil (30 micron) mono-axially oriented, ethylene tetrafluoroethylene (ETFE) film. It offers superior weather ability, UV transmission, chemical and graffiti resistanc.. |
|||
Thickness | 30.5 microns | 1.20 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 30 ARW OPP Film Product Description: Bicor ARW is a two-side acrylic coated OPP film designed for use in lamination and monoweb applications, especially for paper ream wrap. The acrylic-coated side with the higher .. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 120 XRG-2 OPP Film Product Description: Bicor 120 XRG-2 is a one-side sealable OPP film that can be used as the inside web of a lamination where exceptional seal performance is required. The high-energy surface is int.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 30MB400 OPP Film Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina.. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Hicor® 30 HF 104 OHD Film One-side sealable, one-side treated, coextruded, oriented high density polyethylene film. It is ideal for use in HFFS and VFFS machines. It is designed to be used unsupported or in laminated applic.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Label-Lyte® 30 LLG-101 Clear OPP Film Product Description: A clear, one-side treated, biaxially oriented polypropylene film that is used in roll-fed labeling. This film can be laminated to itself (at other gauges of LLG-101) or applied .. |
|||
Thickness | 30.5 microns | 1.20 mil | |
ExxonMobil Label-Lyte® 30 XU-001 Clear OPP High-shrink Film Clear, high-shrink film designed for use in roll-fed labeling of contoured containers such as aluminum and steel beverage cans, beaded metal cans, aerosol containers, and contoured glass and plastic.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 30LL666 OPP Film Product Description: A transparent, high gloss, two side acrylic coated BOPP film for reel-fed wrap-around labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |
|||
Thickness | 30.5 microns | 1.20 mil | Nominal; ExxonMobil Method |
ExxonMobil Bicor® 120 SLP OPP Film Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Bicor™ 30MBT666 OPP Film Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M 5836 Clean-Walk Unframed Mat 3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adh.. |
|||
Thickness | 30.5 microns | 1.20 mil | Facestock |
3M FP08R2 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 30.5 microns | 1.20 mil | Facestock |
3M FP531 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3721 Industrial Cold Temperature Box Sealing Tape Scotch® Box Sealing Tape 3721 is an industrial cold temperature packaging tape for use at refrigeration temperatures, or at room temperature with subsequent storage at low temperatures. This produc.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3771 Standard Message Box Sealing Tape Scotch® Box Sealing Tape 3771 is a standard message packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consist.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3779 Security Message Box Sealing Tape Scotch® Security Message Box Sealing Tape 3779 is an industrial packaging tape used for box sealing specifically where security of the carton contents is a concern. The printed design along with th.. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M 5830 Clean-Walk Unframed Mat 3M™ Clean-Walk Unframed Mats 5830 Series are a multi-sheeted adhesive system that removes dirt and contaminates from shoe soles, wheels and other passing objects on contact. Comprised of a thin adh.. |
|||
Thickness | 30.5 microns | 1.20 mil | Adhesive |
3M 7847 Laser Markable Label Material 3M™ Laser Markable Label Material 7847 and 7848 are specialty film label materials where a laser can ablate the top layer of a dual-layer facestock to create an image. The same laser can also kiss .. |
|||
Thickness | 30.5 microns | 1.20 mil | Backing; ASTM D3652 |
3M Scotch® 3781 Industrial Continuous Taping System Tape Scotch® Taping System Tape 3781 is an industrial continuous packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. The Product .. |
|||
Thickness | 30.5 microns | 1.20 mil | Adhesive |
3M 8418 Polyester Film Tape 3M™ Polyester Film Tape 8417 is a self-wound (linerless) transparent polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. It is often used as an overlaminate in conjunction with 3.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 30 HM-3 OPP Film Product Description: A white opaque OPP film with a proprietary cavitated core. HM-3 is designed for cold seal applications and is used as a surface print, monoweb, or as the inside of lamination. I.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 30MD447 OPP Film Product Description: A coextruded super white opaque, modified higher density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for u.. |
|||
Thickness | 30.5 microns | 1.20 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 30MW747 OPP Film Product Description: White opaque biaxially oriented polypropylene film coated on one side acrylic, one side PVdC. Provides excellent performances on all packaging machines. 30MW747 is a super white.. |