Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-131 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-15 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-186 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-196 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-37 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-59 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-99 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-10 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-105 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-11 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-13 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-17 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-176 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-186 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-197 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-27 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-66 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-89 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-307 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-54 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-98 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-130 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-139 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-357 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-48 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-59 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-131 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |